Written by James Hill
Quick answer: A filament data sheet tells you three things: how to print the material (temperatures, speed, drying), what the plastic is like (density, moisture absorption, melt flow) and how test parts perform (strength, stiffness, stretch, impact and heat resistance). Only compare figures measured to the same standard, load and print orientation.
Most OzFDM filament pages have a downloadable PDF technical data sheet. A figure like "45.5~49 MPa" means little until you know what was tested, so this guide walks through every field on our sheets using real values from our PLA+, PETG+, TPU95A, ASA-GF and PPA-CF listings, then explains why the same material can score differently between brands.
Where to find the data sheet
Scroll to Technical Specifications on any filament product page. The figures are grouped into Product Specifications, Print Parameters, Mechanical, Physical and Thermodynamic Properties, with Electrical Characteristics on some engineering grades. The PDF on the same page carries the same figures, sometimes with extra handling notes, and ends with a reminder that "values shown are typical results measured on test specimens and are provided for guidance only". A data sheet describes test bars, not your part.
Product specifications: the roll itself
| Field | What it tells you | OzFDM example |
|---|---|---|
| Filament diameter | The nominal diameter for your slicer profile | 1.75 mm |
| Dimensional tolerance | How far the diameter can vary along the roll. Tighter tolerance gives more consistent extrusion | ±0.03 mm for PLA+ and PETG+; ±0.05 mm for TPU95A, ASA-GF and PPA-CF |
| Filament weight | Net weight of filament, not counting the spool | 1 kg |
| Spool weight (empty and new) | Weigh a part-used roll and subtract the empty spool to see how much filament is left | 150 g empty, 1.15 kg new |
| Spool diameters and width | Check the spool fits your AMS, spool holder or dryer | 200 mm outer, 52 mm hub, 65 mm wide |
| Package weight and dimensions | Boxed shipping size | 1.3 kg, 210 x 220 x 75 mm |
| Colour hex codes | An approximate on-screen colour for planning multicolour prints | PLA+ Black is listed as #1B1B18 |
Print parameters and drying
Temperatures and speeds are given as ranges, sometimes with a recommended value in brackets. Start at the recommended value, or mid-range, and fine-tune with a temperature tower. Support material lists what separates cleanly from the filament, and the storage recommendation is an airtight bag or container with desiccant.
| Filament | Nozzle | Bed | Speed | Drying |
|---|---|---|---|---|
| PLA+ | 190–220°C | 25–60°C | 60–90 mm/s | 40–45°C for 4–6 hours |
| PETG+ | 210–230°C | 50–70°C | 40–60 mm/s | 70°C for 5 hours |
| TPU95A | 200–240°C (230°C recommended) | 20–60°C (40°C recommended) | 30–150 mm/s (60 mm/s recommended) | 70°C for at least 5 hours |
| ASA-GF | 240–260°C (250°C recommended) | 100–120°C (110°C recommended) | 40–250 mm/s | 80°C for at least 5 hours |
| PPA-CF | 255–275°C (270°C recommended) | 80–100°C (90°C recommended) | 60–250 mm/s (200 mm/s recommended) | 120°C for at least 8 hours (PDF data sheet) |
Note that the PLA+ drying temperature sits below its 53°C heat deflection temperature: dry a roll hotter than the plastic can take and it distorts on the spool. Notes such as "hardened steel nozzle required" on PPA-CF are not optional, because abrasive fibre-filled materials wear brass nozzles quickly.
Physical properties
| Field | Test standard | What it means | OzFDM examples |
|---|---|---|---|
| Density | ISO 1183 | Mass per volume in g/cm³. Lower density gives more metres per kilogram and lighter parts | PLA+ 1.25–1.26; PETG+ 1.27–1.28; ASA-GF 1.17–1.18; PPA-CF 1.21–1.23 |
| Melt flow rate (MFR) | ISO 1133 | Grams of molten plastic pushed through a standard die in 10 minutes at a set temperature and weight. Higher flows more easily; compare only at the same conditions | PLA+ 3–6 g/10 min at 190°C and 2.16 kg; PETG+ 8–12 at 220°C and 2.16 kg; PPA-CF 35–40 at 280°C and 5 kg |
| Moisture absorption | ISO 62 | Weight gained after 24 hours at 23°C under the standard's test conditions. Higher numbers mean the material needs drying more often | PETG+ under 0.2%; PLA+ under 0.3%; TPU95A under 0.5%; PA6 Nylon 1.6–1.9% |
Density is also why two 1 kg rolls are not the same length. At 1.75 mm, a kilogram of filament at 1.25 g/cm³ is about 333 m long, while at 1.17 g/cm³ it is about 355 m.
Mechanical properties
These come from standard test bars pulled, bent or struck in a machine. 1 MPa is one newton on each square millimetre.
| Field | ISO standard (common ASTM equivalent) | What it measures | OzFDM examples |
|---|---|---|---|
| Tensile strength | ISO 527 (ASTM D638) | The highest stress a bar takes while being pulled apart | PLA+ 45.5–49 MPa; PETG+ 41–45 MPa; PPA-CF 108–112 MPa (X-Y) |
| Elongation at break | ISO 527 (ASTM D638) | How far the bar stretches before breaking, as a percentage. Low means brittle | PPA-CF 3.5–5%; PLA+ 14.5–16.5%; TPU95A 800–1,000% |
| Tensile modulus | ISO 527 (ASTM D638) | Stiffness when pulled: how hard it is to stretch a little, not how hard it is to break | TPU95A 6–7 MPa; PLA+ 950–1,050 MPa; PPA-CF 7,100–8,000 MPa (X-Y) |
| Flexural strength | ISO 178 (ASTM D790) | The highest bending stress the bar takes | PLA+ 73–76 MPa; ASA-GF 72.5–74.1 MPa (X-Y) |
| Flexural modulus | ISO 178 (ASTM D790) | Stiffness in bending: how much a bracket or panel will flex | ASA-GF 3,359–3,368 MPa (X-Y); PPA-CF 6,500–7,000 MPa (X-Y) |
| Impact strength (Izod) | ISO 180 (ASTM D256) | Energy absorbed when a pendulum strikes a bar held at one end. ISO gives kJ/m², ASTM usually J/m, so they do not convert directly | PLA+ 9.5–10.5 kJ/m²; PPA-CF 9–11 kJ/m² (X-Y); TPU95A "NB", meaning no break |
| Shore hardness | ISO 7619-1 (ASTM D2240) | Resistance to indentation, 0 to 100. Shore A is for softer materials, Shore D for harder ones, with no simple conversion between them | TPU95A: 95A |
Strength, stiffness and toughness are different things
Tensile strength is not a measure of how good a filament is. PPA-CF has more than twice the tensile strength of PLA+ and seven to eight times the tensile modulus, but stretches only 3.5–5% before breaking. For a snap-fit clip, elongation matters more than strength. For a bracket that must not sag, look at flexural modulus. For a part that gets dropped, look at impact strength and elongation together.
X-Y, X-Z and Z figures
Some of our engineering sheets give figures for more than one direction. X-Y values are measured along the printed layers, in the plane of the build plate. Z and X-Z values put more of the load across layer lines, where the bond between layers limits strength, and the gap is large. PPA-CF lists flexural strength of 210–221 MPa in X-Y but 70–75 MPa in Z, and impact strength of 9–11 kJ/m² in X-Y but 2.5–3 kJ/m² in Z. ASA-GF lists flexural strength of 72.5–74.1 MPa in X-Y and 27.2–31.7 MPa in X-Z. If a sheet gives one figure, assume it is the best direction, and orient loaded parts so force runs along the layers.
Thermal properties
Heat deflection temperature (HDT)
HDT is measured under ISO 75 or ASTM D648. A test bar is loaded in three-point bending and heated at 2°C per minute until it bends by a small set amount (0.25 mm in ASTM D648). Two loads are common: 0.45 MPa (66 psi) and 1.8 MPa (264 psi). The heavier load gives a lower result, so an HDT figure means nothing without its load. Our listings use 0.455 MPa, except PA12-CF, which is listed at 1.8 MPa. Examples: PLA+ 53°C, PETG+ 68°C, ASA-GF 88°C and PPA-CF 220°C. Every material we sell is compared in our filament heat resistance chart.
Vicat softening temperature
You will see Vicat on many other brands' sheets. The Vicat test (ISO 306 or ASTM D1525) pushes a flat-ended needle with a 1 mm² tip into the sample under a 10 N (method A) or 50 N (method B) load while heating it, and records the temperature at which the needle sinks 1 mm. It measures surface softening under a point load, not a bar bending, so never compare one brand's Vicat with another's HDT. Our listings do not currently include Vicat.
Continuous use temperature
Many of our sheets also list a continuous use temperature. Most use IEC 60216, the standard for long-term thermal endurance, and a few cite UL 746B (RTI) or a typical published value for the base polymer, with the source named next to the figure. It describes long exposure rather than a short heating ramp: PLA+ 50°C, PETG+ 65°C and PPA-CF 120°C. For a part that sits warm for months, read it alongside HDT.
Electrical and fire ratings
Surface resistance (IEC 60093) appears on some of our carbon fibre engineering grades and is the key figure for anti-static materials. It is measured in ohms, and lower means the surface carries charge away more readily; PPS-CF, for example, lists 10⁵ Ω or less, and PA12-CF adds insulation resistance to IEC 60167. Flame retardancy to UL 94 appears on flame-retardant grades. V-0 is the most demanding of the V-0, V-1 and V-2 vertical burn ratings, and a rating only applies at the thickness tested: our ABS-FR lists V-0 at 1.5 mm.
Why values differ between brands
Two PLA+ sheets can disagree widely without either being wrong. Check these points before comparing.
| Check | Why it changes the number |
|---|---|
| Test standard | ISO and ASTM methods use different specimen shapes, test speeds and units |
| Specimen type | Some brands test injection-moulded bars with no layer lines. Printed bars usually score lower, and print settings change the result |
| Print orientation | As the PPA-CF figures show, strength across layers can be a third of the strength along them |
| HDT load | 0.45 MPa and 1.8 MPa results for the same material are different numbers |
| Conditioning | Dry and moisture-conditioned specimens test differently, especially nylon |
| Annealing | Annealed and as-printed specimens differ. Our PPA-CF data sheet suggests annealing at 80–100°C for 1–3 hours |
| Typical or minimum values | Our sheets give typical ranges. Some manufacturers publish guaranteed minimums, others a single typical value |
How to use a data sheet to choose a filament
- Start with the conditions. Use HDT and continuous use temperature to rule out materials that will soften where the part lives.
- Match the property to the likely failure. Flexural modulus for sagging, elongation and impact strength for cracking, Shore hardness for grip.
- Check you can print it. Compare temperatures with your printer's limits and note any hardened nozzle, enclosure or drying requirement.
- Shortlist, then test. Our Filament Finder narrows the range, then print the real part.
Shop the materials in this guide
- 1.75 mm PLA+ Filament, 1 kg: the everyday baseline used for most examples in this guide
- 1.75 mm PETG+ Filament, 1 kg: 68°C HDT and low moisture absorption for general functional parts
- 1.75 mm TPU95A Filament, 1 kg: 95A Shore hardness and 800–1,000% elongation for flexible parts
- 1.75 mm ASA-GF Filament, 1 kg: glass fibre ASA with separate X-Y and X-Z figures on its sheet
- 1.75 mm PPA-CF Filament, 1 kg: 220°C HDT and high stiffness for demanding engineering parts
Frequently asked questions
What does HDT mean on a filament data sheet?
Heat deflection temperature: the point at which a loaded test bar bends by a set amount as it heats. Use it to compare materials at the same load, not as a safe working temperature.
What does 95A mean on TPU?
A Shore A hardness of 95, near the firm end of the scale used for rubbery materials. Lower Shore A numbers are softer.
Why are my printed parts weaker than the data sheet?
Data sheet values come from standard test bars, often printed solid in the best orientation or injection moulded. Real parts have infill, layer lines in the load path and sometimes damp filament, all of which lower the result.