Written by Jackson B.
Quick answer: TPU 95A is the tougher, stretchier option, with Shore 95A hardness, 800–1000% elongation and 30–150 mm/s on our data sheet. Flexible PLA prints at PLA temperatures but slowly (10–30 mm/s), and lists a 53°C HDT with no mechanical figures yet. Keep both out of the Bambu AMS and AMS lite. On a Bowden printer, start with Flexible PLA.
Flexible PLA and TPU 95A both make parts that bend, squash and spring back, and both come on 1 kg spools in 14 colours. They are not interchangeable, though. They print at different speeds, suit different extruders and fit different jobs. At the time of writing, a roll of Flexible PLA is $27.95 and a roll of TPU95A is $34.95.
This comparison uses the figures on our data sheets and product pages to cover the numbers, printer and AMS compatibility, which filament fits which application, and starting settings for each.
The data sheets side by side
| Property | Flexible PLA | TPU95A |
|---|---|---|
| Base material | Modified, elastic PLA made from PBAT-based raw materials | Thermoplastic polyurethane |
| Shore hardness (ISO 7619-1) | Not listed | 95A |
| Elongation at break (ISO 527) | Not listed | 800–1000% |
| Tensile strength (ISO 527) | Not listed | 27–28 MPa |
| Tensile modulus (ISO 527) | Not listed | 6–7 MPa |
| Nozzle temperature | 180–220°C | 200–240°C (230°C recommended) |
| Bed temperature | 25–60°C | 20–60°C (40°C recommended) |
| Print speed | 10–30 mm/s | 30–150 mm/s (60 mm/s recommended) |
| HDT (ISO 75, 0.455 MPa) | 53°C | 95°C |
| Density | 1.25–1.26 g/cm³ | 1.2–1.25 g/cm³ |
| Diameter tolerance | ±0.03 mm | ±0.05 mm |
| Drying | 60°C for 6 hours or more | 70°C for at least 5 hours |
The Flexible PLA listing no longer publishes mechanical figures. The values it used to carry had been copied across from a thermoplastic polyurethane and did not describe the material, so they have been removed and verified figures are still to come. That leaves print speed, hardness and heat resistance as the properties the two sheets can actually be compared on, and TPU95A leads on all three.
On heat, Flexible PLA lists 53°C, the same as our standard PLA grades, so keep it out of hot places. TPU95A lists 95°C, although HDT is a rigid bar test and only a rough guide for a flexible material. If a flexible part will live somewhere hot, test it first, and see our guide to choosing filament for a hot car.
How each one behaves
Flexible PLA
Our product page describes Flexible PLA as combining the ease of printing PLA with rubber-like flexibility. It bends, compresses and returns to shape, with a controlled level of flexibility that keeps enough structure for practical parts. It has a softer feel than rigid filament, and the page notes it is slightly more demanding to print than standard PLA. The trade-off is speed: 10–30 mm/s is slow, so larger parts take a long time.
TPU95A
At Shore 95A, our TPU95A is firm enough to hold its shape under load and soft enough to absorb shock, vibration and repeated bending. The product page highlights resistance to tearing, compression fatigue and impact, and resistance to oils, greases and many solvents. It has a satin matte finish. Its listed speed range is also much wider, with 60 mm/s recommended and up to 150 mm/s on the data sheet, although the product page still advises slow speeds for best results.
AMS, AMS lite and Bowden compatibility
Feeding is where flexible filament succeeds or fails. Soft filament can compress or buckle anywhere it is pushed through a long path, so the shorter and more direct the path, the better.
| Feed setup | Flexible PLA | TPU95A |
|---|---|---|
| Direct drive extruder | Yes, at 10–30 mm/s | Yes, the setup our product page describes |
| Bowden extruder | Our product page says it does not need a specialised direct drive setup | Start with Flexible PLA instead |
| Bambu AMS or AMS 2 Pro | Not recommended | Not recommended |
| Bambu AMS lite | Not recommended | Not recommended |
| External spool holder or dry box | Recommended | Recommended |
Our product pages for both filaments advise against the AMS and recommend feeding from an external spool. Bambu Lab agrees. Its TPU printing guide says 77D and 55D TPU can run through the AMS, 95A, 85A, 83A and 80A may bend inside it, and 75A or softer should not be printed on Bambu printers at all. The AMS lite FAQ says to avoid flexible materials including TPU and TPE.
For external feeding, Bambu suggests putting dried TPU in a sealed box with a roller axle and fresh desiccant, because the roller reduces the resistance the extruder has to pull against. Our guide to OzFDM filament in the Bambu AMS has more on spools and presets, and Direct Drive vs Bowden explains why the extruder layout matters.
Which one for which job
| Application | Better pick | Why |
|---|---|---|
| Gaskets and seals | TPU95A | Resistance to oils, greases and many solvents is listed on its product page |
| Vibration dampers, feet and bumpers | TPU95A | Built to absorb shock and vibration and resist compression fatigue |
| Hinges and couplings | TPU95A | Named on its product page for parts in repeated motion |
| Phone cases and protective covers | Either, TPU95A for hard wear | Both product pages list phone cases, and the TPU95A page highlights tear and wear resistance |
| Grips, wearables and soft-touch parts | Flexible PLA | Its product page highlights a softer finish for grips and wearable items |
| RC tyres | Flexible PLA | Named in the Flexible PLA product description |
| Any flexible part on a Bowden printer | Flexible PLA | No specialised direct drive setup needed |
Starting settings
These starting points come from our data sheets, with extra TPU values from our TPU on Bambu Lab X1 Carbon print profile. Where a value is not published, we say so rather than guess. To turn them into a slicer preset, follow our guide to creating filament presets in Bambu Studio, OrcaSlicer and PrusaSlicer.
| Setting | Flexible PLA | TPU95A |
|---|---|---|
| Nozzle temperature | 180–220°C | 230°C (range 200–240°C) |
| Bed temperature | 25–60°C | 40°C (range 20–60°C) |
| Print speed | 10–30 mm/s | 30–60 mm/s in our X1 Carbon profile (data sheet allows up to 150 mm/s) |
| First layer speed | Not published, stay at the slow end of the range | 15–20 mm/s |
| Part cooling fan | Not published | 30–60%, off for the first layer |
| Retraction | Not published | 0.4 mm at 30 mm/s, kept to a minimum |
| Drying before printing | 60°C for 6 hours or more | 70°C for at least 5 hours |
| Support material | PVA as a support interface | PVA |
| Feed | External spool | External spool |
Settings sources: OzFDM Flexible PLA and TPU95A data sheets and our TPU on Bambu Lab X1 Carbon print profile.
Fixing common problems on your first flexible prints
Our X1 Carbon profile notes that almost every TPU failure is a feed problem rather than a temperature one. The filament buckles somewhere between the drive gear and the melt zone, so slow down and check the feed path before you touch temperatures. The same logic applies to Flexible PLA, which our product page says prints best at lower speeds so the material flows without buckling or resistance in the feed path.
- Filament grinds or stops feeding. Print slower and reduce extruder tension if your printer allows it. Flexible filament cannot be pushed the way a rigid filament can.
- Blobs and zits on the surface. Retraction is usually too long. Our TPU profile suggests 0.4–0.8 mm, because long retractions stretch the filament instead of pulling it back.
- Gaps between perimeters. Increase flow by 2–3%. Soft filament compresses slightly in the drive gear, so it can under-extrude at default flow.
- Stringing. Bambu's TPU guide notes that TPU is prone to stringing and advises against excessive travel moves. Dry the roll first, since damp filament strings more.
- Feeding trouble with a third-party preset. For TPU without its own profile, Bambu suggests starting from the generic TPU preset with a lower maximum volumetric speed.
Shop the materials in this guide
- 1.75 mm Flexible PLA Filament - 1 KG: soft-touch flexible parts at PLA temperatures, and the easier choice on Bowden printers.
- 1.75 mm TPU95A Filament - 1 KG: Shore 95A for dampers, gaskets, hinges and hard-wearing covers.
- Flexible Filament: both flexible ranges in one place.
- 1.75 mm PVA Support Filament - 0.5 KG: the support material listed on both data sheets.
- Filament Drybox Roller Insert: roller wheels and desiccant trays that turn a clip-lock container into a feed box for an external spool.
Frequently asked questions
Is Flexible PLA softer than TPU 95A?
We cannot say from the data sheets. The Flexible PLA sheet lists neither a Shore hardness nor an elongation figure, so there is nothing to set against TPU95A's Shore 95A and 800–1000% elongation.
Can I print TPU 95A on a Bowden printer?
Our TPU95A product page describes feeding through a direct drive extruder, so that is the setup we recommend. On a Bowden printer, start with Flexible PLA, which its product page says does not need a specialised direct drive setup.
Can either filament go in the Bambu AMS?
We do not recommend it for either. Soft filament can buckle in the feed tubes and jam. Bambu's TPU guide says 95A TPU may bend inside the AMS, and the AMS lite FAQ says to avoid TPU and TPE. Feed both from an external spool.
Which handles heat and chemicals better?
TPU95A. It lists a much higher HDT (95°C against 53°C) and resistance to oils, greases and many solvents. Flexible PLA sits at standard PLA heat resistance and is positioned for indoor use.
Do I need to dry flexible filament?
Dry it before long prints, especially once a roll has been opened. Our data sheets recommend 60°C for 6 hours or more for Flexible PLA and 70°C for at least 5 hours for TPU95A.