High Speed PLA on Bambu Lab X1 Carbon

OzFDM High Speed PLA 1.75 mm filament for the Bambu Lab X1 Carbon

Written by Jackson B.

Recommended slicer settings for OzFDM High Speed PLA on the Bambu Lab X1 Carbon.


Nozzle Temp

215 °C

Range: 190 – 220 °C

Bed Temp

55 °C

Range: 25 – 60 °C

Print Speed

200

mm/s · max 300

Layer Height

0.20

mm · max 0.28

Fan Speed

100 %

1st layer: 0 %

1st Layer Speed

30

mm/s

Retraction

0.8 mm

@ 30 mm/s

Nozzle Type

Hardened

Stock 0.4 mm


Retraction Note

  • The default 0.8 mm retraction is enough at speed. Increase it in 0.2 mm steps only if stringing continues after drying the filament.


Full Settings Reference

Settings

Recommended

Range

Nozzle Temperature

210 – 220 °C

190 – 220 °C

Bed Temperature

50 – 60 °C

25 – 60 °C (lower end on a Cool Plate)

Print Speed

150 – 300 mm/s

data sheet: 60 – 350 mm/s

First Layer Speed

30 mm/s

slower is better for adhesion

Layer Height

0.16 – 0.24 mm

0.12 – 0.28 mm

Fan Speed (Normal)

100 %

Fan Speed (1st Layer)

0 %

Retraction Distance

0.8 mm

Direct drive

Retraction Speed

30 mm/s

Nozzle Type

Hardened steel (stock)

any 0.4 mm nozzle suits this material

Dry Filament

40 – 45 °C for 4 – 6 h

store sealed with desiccant between prints

Enclosure

Not required

open the door and remove the top glass on long prints

Support Material

PVA, PETG (interface)


Printing Notes

High Speed PLA is a toughened PLA made to melt and extrude evenly at speed, so it suits Bambu Studio's faster process presets better than standard PLA.

Faster printing needs more heat. Run nearer 210 °C at moderate speeds and nearer 220 °C at the top of the speed range, but do not go past 220 °C.

Speed is also capped by the max volumetric speed in the filament preset. If fast prints show gaps or rough walls, the hotend has run out of flow, so lower the speed.

The X1C has no chamber heater, but bed heat builds up with the door shut. Bambu Lab recommends opening the front door and removing the top glass when the bed runs above the filament's softening point, so do this for long PLA prints at 55 – 60 °C.

Slicer: Bambu Studio. Start from the Generic PLA filament preset and set the temperatures above. Every figure assumes dry filament, so dry at 40 – 45 °C for 4 – 6 h before a long print.

Tested on our Bambu Lab X1 Carbon with a 0.4 mm nozzle, September 2026.

Troubleshooting

Gaps in walls or thin top layers at speed: Flow limit reached. Drop the print speed by about 20 % or raise the nozzle to 220 °C.

Ripples beside sharp corners: This is motion, not filament. Lower the outer wall speed and leave inner walls and infill fast.

Warped corners on long flat parts: Wash the plate with warm water and dish soap, raise the bed to 60 °C and slow the first layer to 20 mm/s.


OzFDM High Speed PLA Filament

  • Toughened PLA built for fast printers, with clean detail and strong layers at speed.

Shop OzFDM High Speed PLA filament

Shop the materials in this guide